MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Murtfeldt Material ”S”® 1000 Black Antistatic Polyethylene, Conductive
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compression-molded at high pressure and temperatures to form new semi-finished products. This results in a high-quality material with an exceptional price/performance ratio that is characterized by exceptional abrasion resistance and good slide properties.

Special Properties:
• Physiologically safe
• Good wear resistance properties
• Good slide properties
• Good anti-adhesion properties
• No moisture absorption
• Antistatic

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: PE-UHMW
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density <= 0.940 g/ccISO 1183
Moisture Absorption at Equilibrium <= 0.010 %ISO 62
Water Absorption at Saturation <= 0.010 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64DIN 53505
Ball Indentation Hardness 38.0 MPa
Tensile Strength 24.6 MPaISO 527
Tensile Strength, Yield >= 15.0 MPaISO 527
Elongation at Break 230 %ISO 527
Modulus of Elasticity 0.950 GPa
Compressive Yield Strength 6.00 MPa
@Strain 1 %
ISO 604
 10.5 MPa
@Strain 2 %
ISO 604
 18.0 MPa
@Strain 5.0 %
ISO 604
Charpy Impact, Notched >= 140 kJ/m²ISO 179
Coefficient of Friction, Dynamic 0.10 - 0.20
Sand Slurry 120value in %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 1.00e+6 ohm-cmIEC 60093
Surface Resistance <= 1.00e+9 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 23.0 - 60.0 °C
Thermal Conductivity 0.400 W/m-KISO 52612
Melting Point 130 - 135 °CISO 3146
Maximum Service Temperature, Air 90.0 °CShort Term
 80.0 °C
@Time 1.80e+7 sec
Minimum Service Temperature, Air -150 °C
Glass Transition Temp, Tg -120 °C
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA No
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive
Sanyo PELESTAT® NC7530 Antistatic Additive
Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive
Plastcom SLOVAMID® 6 GF 30 AS PA6 reinforced with glass fiber, anti-static agent
Sanyo J-STAT 3180 Antistatic Additive

PMURT906 / 156553

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.