System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Sanyo J-STAT 3180 Antistatic Additive
Categories:
Other Engineering Material
;
Additive/Filler for Polymer
;
Polymer
Material Notes:
Information provided by Tomen America, a US distributor of Pelestat.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Additive Loading
18 - 23 %
18 - 23 %
to achieve surface resistivity=10^11 ohms
Melt Flow
70
g/10 min
@Load 2.16 kg,
Temperature 230 °C
70
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Electrical Properties
Metric
English
Comments
Surface Resistance
5.00e+9
ohm
5.00e+9
ohm
kept at 23°C under 50% R.H.
Thermal Properties
Metric
English
Comments
Melting Point
160
°C
320
°F
Maximum Service Temperature, Air
270
°C
518
°F
Degradation Temp
Descriptive Properties
Appearance
Pale Yellow Pellet
Applicable Thermoplastic
PP
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive
Murtfeldt Material ”S”® 1000 Black Antistatic Polyethylene, Conductive
Plastcom SLOVAMID® 6 GF 30 AS PA6 reinforced with glass fiber, anti-static agent
Arkema Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® MH 1657 Polyether Block Amide (PEBA)
PSANYO06 / 66530
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.