MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ohio Carbon Blank OCB AR-12 EDM Grade Graphite
Categories: Carbon; Graphite

Material Notes: Available in a range of sizes and shapes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 1.78 g/cc0.0643 lb/in³
Particle Size 7.9 µm7.9 µmAverage
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363
Tensile Strength 29.5 MPa4280 psi
Flexural Strength 52.0 MPa7540 psi
Compressive Strength 106 MPa15400 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00135 ohm-cm0.00135 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 89.9 W/m-K624 BTU-in/hr-ft²-°F
 
Descriptive Properties
GrainSuper-Fine
Suggested ApplicationsForging Dies
 Large Cavity Molds
 Large Die Casts
 Large Extrusion Dies
 Roughing Electrodes
Wear ResistanceGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CoorsTek CRB-100 Resin-Impregnated Carbon Graphite
Graphite, Carbon, C
LKAB Minerals FireCarb TEG-315 Expandable Graphite
NeoGraf eGRAF® HITHERM™ HT-720 Graphite
Schunk FH42Y3 Carbon Graphite

EOHIOCA72 / 108536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.