MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NeoGraf eGRAF® HITHERM™ HT-720 Graphite
Categories: Carbon; Graphite

Material Notes: Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ material is offered in a variety of through thickness thermal conductivities, available in roll or die-cut form and can be laminated with plastics and adhesives. An economical thermal interface material, HITHERM™ products will not dry out and no outgassing occurs under vacuum conditions. The conformability of HITHERM™ materials optimizes thermal properties, ensures excellent contact, and is maintained for the life of the assembly. Typical applications include thermal interfaces, chip burn-in, chip testing fixtures, DC-to-DC converters, CPU modules, microprocessors, and hot and cold plates.

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 508 microns20.0 mil
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00100 ohm-cm0.00100 ohm-cmIn-Plane
 1.50 ohm-cm1.50 ohm-cmThrough Thickness
 
Thermal PropertiesMetricEnglishComments
CTE, linear -0.400 µm/m-°C-0.222 µin/in-°FIn-Plane
 27.0 µm/m-°C15.0 µin/in-°FThrough Thickness
Specific Heat Capacity 0.711 J/g-°C0.170 BTU/lb-°F
Thermal Conductivity 6.00 W/m-K41.6 BTU-in/hr-ft²-°FThrough Thickness; ASTM-D5470 Modified (at 110kPa/16 psi/1.1 bar)
 240 W/m-K1670 BTU-in/hr-ft²-°FIn-Plane; Angstrom's Method
Maximum Service Temperature, Air 400 °C752 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NeoGraf eGRAF® HITHERM™ HT-1220 Graphite
NeoGraf eGRAF® HITHERM™ HT-705 Graphite
NeoGraf eGRAF® SPREADERSHIELD™ SS300 Graphite
NeoGraf eGRAF® HITHERM™ HT-1205 Graphite
NeoGraf eGRAF® HITHERM™ HT-2505 Graphite with Polymer Additive

CGRAF916 / 107320

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.