MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Telcar® TELC 3050 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Telcar TELC 3050 is a general purpose thermoplastic elastomer, available in NAT and BLK, designed for industrial and electrical applications requiring flexibility over a wide temperature range. Telcar TELC 3050 is a high durometer grade that is RoHS compliant. This grade is UL listed and is suitable for both injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Bondability; Chemical Resistant; Good Adhesion; Good Colorability; Good Processability; Good Tear Strength; Good Toughness; High Hardness; Low Density; Low Flow; Low Specific Gravity; Without Fillers

Uses: Building Wire Insulation; General Purpose; Industrial Applications; Profiles; Rubber Replacement; Wire & Cable Applications; Wire Jacketing

Agency Rating: UL Unspecified Rating

RoHS Compliant:RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D792
Viscosity 501 cP
@Shear Rate 206 1/s,
Temperature 200 °C
501 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 48
@Time 5.00 sec
48
@Time 0.00139 hour
ASTM D2240
 51.3
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
51.3
@Treatment Temp. 230 °F,
Time 1008 hour
Change in Air; ISO 188
Tensile Strength at Break 11.7 MPa1700 psiFlow; ASTM D412
 12.1 MPa1750 psiAcross Flow; ASTM D412
 13.0 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
1880 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
 13.2 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
1910 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tensile Strength  8.03 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
1160 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
 8.18 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
1190 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  8.14 MPa
@Strain 100 %
1180 psi
@Strain 100 %
Across Flow; ASTM D412
 10.1 MPa
@Strain 100 %
1460 psi
@Strain 100 %
Flow; ASTM D412
Elongation at Break 530 %530 %Flow; ASTM D412
 640 %640 %Across Flow; ASTM D412
Flexural Modulus 0.276 GPa40.0 ksiASTM D790
Tear Strength 90.8 kN/m518 pliAcross Flow; Die C; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.3
@Frequency 1000 Hz
3.3
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 188 - 210 °C370 - 410 °FInjection, Melt
Rear Barrel Temperature 171 - 193 °C340 - 380 °FInjection
Middle Barrel Temperature 177 - 199 °C350 - 390 °FInjection
Front Barrel Temperature 182 - 204 °C360 - 400 °FInjection
Nozzle Temperature 188 - 210 °C370 - 410 °FInjection
Zone 1 166 - 199 °C330 - 390 °FExtrusion
Zone 2 177 - 204 °C350 - 400 °FExtrusion
Zone 3 182 - 210 °C360 - 410 °FExtrusion
Zone 4 182 - 216 °C360 - 420 °FExtrusion
Zone 5 188 - 221 °C370 - 430 °FExtrusion
Die Temperature 190 - 210 °C374 - 410 °FExtrusion
Mold Temperature 25.0 - 65.6 °C77.0 - 150 °FInjection
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Natural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1626 / 238117

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.