Telcar TELC 3050 is a general purpose thermoplastic elastomer, available in NAT and BLK, designed for industrial and electrical applications requiring flexibility over a wide temperature range. Telcar TELC 3050 is a high durometer grade that is RoHS compliant. This grade is UL listed and is suitable for both injection molding and extrusion. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Bondability; Chemical Resistant; Good Adhesion; Good Colorability; Good Processability; Good Tear Strength; Good Toughness; High Hardness; Low Density; Low Flow; Low Specific Gravity; Without Fillers Uses: Building Wire Insulation; General Purpose; Industrial Applications; Profiles; Rubber Replacement; Wire & Cable Applications; Wire Jacketing Agency Rating: UL Unspecified Rating RoHS Compliant:RoHS Compliant Form: Pellets Processing Method: Extrusion; Injection Molding Information provided by Teknor Apex |