MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexMC® C / 2000 / R1 Composite SMC  (discontinued **)
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Composite SMC; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: High performance sheet-molding compound, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume enable components to be molded for a wide range of applications.

Overall Features:

  • Competitive alternative to lightweight alloys (Ti, Al, Mg)
  • Designed for compression molding
  • Rapid processing cycles
  • Complex shapes
  • Molded-in inserts
  • No material waste
  • Internal release agent for multiple demolding
Provided as a 460 mm wide roll; 8 month shelf life at -18° C; 7 day shelf life at RT; Areal weight 2000 g/m²; 57% HS carbon fiber by volume; 2.5 min cure time per mm part thickness.

Information provided by Hexcel Composites.

Key Words: Hexcel Corporation; Carbon Fiber Composite Sheet Moilding Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 300 MPaASTM D638
Tensile Modulus 45.0 GPaASTM D638
Flexural Yield Strength 450 MPaASTM D790
Flexural Modulus 40.0 GPaASTM D790
Compressive Yield Strength 400 MPaASTM D495
Compressive Modulus 35.0 GPaASTM D695
Shear Strength 45.0 MPaI.L.S.S. short beam shear per ASTM D5379
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 88.0 °Cby DMTA following AITM 1-0003. Higher Tg possible by adjustment of cure time.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 135 °CCure Temp

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC
Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC

PHXL00 / 47885

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.