MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® LV-65H FWA black 9225 PA12-GF65
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 50% Glass Fiber Filled

Material Notes: Product description: Grilamid LV-65H FWA black 9225 is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features:
  • High stiffness combined with good toughness
  • High elongation
  • Very low water absorption
  • Hydrolysis and chemical resistance
  • Easy processing, especially suitable for thick-walled moldings
The special composition of Grilamid LV-65H FWA black 9225 makes it suitable for potable water as well as food contact.

Application examples: Grilamid LV-65H FWA black 9225 is designed for applications predominantly in the following application fields:

  • Robust valves and fittings for water and gas supply
  • Taps, fittings, meters, pumps in sanitary equipment
  • Domestic appliances and household goods
  • Components in the food processing industry

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³Dry; ISO 1183
Water Absorption 0.80 %0.80 %Sim. to ISO 62
Moisture Absorption 0.400 %0.400 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85
@Time 15.0 sec
85
@Time 0.00417 hour
Conditioned; ISO 868
Ball Indentation Hardness 185 MPa26800 psiConditioned; ISO 2039-1
Tensile Strength at Break 160 MPa23200 psiConditioned; ISO 527-1/-2
 170 MPa24700 psiDry; ISO 527-1/-2
Elongation at Break 3.0 %3.0 %Dry; ISO 527-1/-2
 3.5 %3.5 %Conditioned; ISO 527-1/-2
Tensile Modulus 17.0 GPa2470 ksiConditioned; ISO 527-1/-2
 18.0 GPa2610 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 35.0 kV/mm889 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 600 V600 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C8.33 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C194 - 248 °FLong Term; ISO 2578
 160 °C320 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 170 °C338 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 140 °C284 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood contact
 
Descriptive Properties
Food contactEU Requirements
 NSF 51
FormGranules
Industry & Consumer goodsHeating systems
 Housewares
 Sanitary, water and gas supply
ProcessingInjection Molding
Product AttributesHydrolysis resistant
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)
Water ContactACS
 DVGW W270
 KTW
 NSF 61
 WRAS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® LBV-65H FWA black 9225 PA12-GF65
EMS-Grivory Grilamid® LV-65H SST black 9288 PA12-GF65
EMS-Grivory Grilamid® LVX-65H SST black 9288 PA12-GF65
EnviroBrass® (SeBiLOY®) III Lead-Free Yellow Brass Casting Alloy, UNS C89550
Overview of materials for Nylon 12, 50% Glass Fiber Filled

PGRH086 / 156795

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.