MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

EnviroBrass® (SeBiLOY®) III Lead-Free Yellow Brass Casting Alloy, UNS C89550
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: The bismuth and selenium additions take the place of lead in this yellow brass. The melting and machining behavior make this alloy a plausible substitute for C85800 in plumbing applications.

Medium section size effect on mechanical properties of castings. Hot tearing in permanent mold castings is much reduced versus leaded yellow brass C85800; no hot tearing was observed for samples with Bi < 1.2%. Does exhibit severe hot tearing when superheat is greater than 234°F (130°C).

Information from the Copper Development Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.40 g/cc0.303 lb/in³estimated from C85800
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  >= 60
@Load 500 kg
>= 60
@Load 1100 lb
Permanent Mold Cast
 63
@Load 500 kg
63
@Load 1100 lb
Typical, Permanent Mold Cast
Tensile Strength, Ultimate >= 240 MPa>= 34800 psiPermanent Mold Cast
 332 MPa48200 psiTypical, Permanent Mold Cast
Tensile Strength, Yield  >= 140 MPa
@Strain 0.5 %
>= 20300 psi
@Strain 0.5 %
Permanent Mold Cast
 200 MPa
@Strain 0.5 %
29000 psi
@Strain 0.5 %
Typical, Permanent Mold Cast
Elongation at Break >= 5.0 %>= 5.0 %Permanent Mold Cast
 8.0 %8.0 %Typical, Permanent Mold Cast
Machinability 75 %75 %at Bi = 0.7%; Permanent Mold Cast; Based on C36000 at 100%
 97 %97 %at Bi = 1.1%; Permanent Mold Cast; Based on C36000 at 100%
 
Thermal PropertiesMetricEnglishComments
Melting Point 860 - 892 °C1580 - 1640 °Fshort freezing range
Solidus 860 °C1580 °F
Liquidus 892 °C1640 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.1 - 0.6 %0.1 - 0.6 %
Antimony, Sb <= 0.05 %<= 0.05 %
Bismuth, Bi 0.6 - 1.2 %0.6 - 1.2 %
Copper, Cu 58 - 64 %58 - 64 %
Iron, Fe <= 0.5 %<= 0.5 %
Lead, Pb <= 0.1 %<= 0.1 %not added intentionally; may be specified lower if required
Nickel, Ni <= 1.0 %<= 1.0 %includes Co content
Other, total <= 0.5 %<= 0.5 %
Phosphorus, P <= 0.01 %<= 0.01 %
Selenium, Se 0.01 - 0.1 %0.01 - 0.1 %
Silicon, Si <= 0.25 %<= 0.25 %
Sulfur, S <= 0.08 %<= 0.08 %
Tin, Sn <= 1.2 %<= 1.2 %
Zinc, Zn 32 - 38 %32 - 38 %
 
Descriptive Properties
BrazingGood
Casting Fluidity25 cm at 100F (56C) superheatRagone Test
DrossingLow
Piping TendencyHigh
Porosity after CastingLower than C85800
SolderingExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Brass Arsenical, UNS C68700
EMS-Grivory Grilamid® LBV-65H FWA black 9225 PA12-GF65
EnviroBrass® (SeBiLOY®) I Lead-Free Casting Alloy, UNS C89510
EMS-Grivory Grilamid® LV-65H FWA black 9225 PA12-GF65
Navy "M" Bronze, UNS C92200, Copper Casting Alloy

NSEBIL905 / 147813

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.