MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik TEGO® RHEO 8500 Thickener
Categories: Other Engineering Material

Material Notes: Product description: TEGO® RHEO 8600 is a non-ionic thickener based on polyurethane

Application: TEGO® RHEO 8600 is a very efficient thickener for dispersions based on acrylates, vinyl-ethylene-copolymers (VAE) and polyvinyl acetate (PVAc). TEGO® RHEO 8600 provides high viscosity in dispersions where standard thickening agents such as acrylates at low pH or polyvinyl alcohols for PVAc/VAE-dispersions fail. Its Newtonian flow behavior is beneficial in applications wherein thick layers need to be applied such as in construction tapes. Additionally, TEGO® RHEO 8600 is very useful, if the adhesive needs to be applied very precisely e. g. in dots without flowing apart. Such applications require a high viscosity that can stand high shear stress.

Properties / Benefits: TEGO® RHEO 8600:

  • is used as thickening agent for water-based systems
  • provides good long term stability
  • shows Newtonian flow behavior
  • is highly efficient even at lower pH-values
  • improves leveling
  • can be combined with other thickeners
  • is solvent free
  • does not contain emulsifiers

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 30000 cPdynamic; DIN 53019
 
Descriptive Properties
Appearanceclear to hazy liquid
Content25%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for 7000 Series Aluminum Alloy
Chemours Teflon® PTFE Grade 304A Aqueous Dispersion
SABIC PVC 673E Emulsion Polyvinyl Chloride
Chemtotal F23 Guar Gum Powder
Chemtotal D.Col FHG290 Guar Gum Powder

PEVONIL561 / 196765

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.