MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemtotal D.Col FHG290 Guar Gum Powder
Categories: Polymer

Material Notes:

Gum of guar is an amazingly versatile and efficient high polymer hydrophilic hydrocolloid, economical in use and easy to handle. Its ability to form highly viscous colloidal dispersions at low concentrations, without heating, makes it one of the most interesting of the hydrocolloids. It is few of naturally available water soluble gums, chemically classified as a galactomannan and possessing a molecular weight reported to be of order 200,000-250,000. It is nontoxic and nonionic, could be used with other synthetic and natural hydrocolloids. One of the most powerful water binder and viscosity enhancer, superior to practically all known water soluble gums.

Properties: Guar Gum powder increase the viscosity of the aqueous base even at small concentration of approximately 1%. Guar based gels are NonNewtonian i.e. their viscosity changes with the change in temperature. It has a Galactose to Mannose ratio of 1:2.. Solubility rates of Guar Gum powder could be increased by choosing an appropriate manufacturing process, thus achieving the Quick/Fast Hydrating Guar grades. It is insoluble in organic solvents and soluble in water(hold and cold). Being nonionic Guar is not effected by pH, but it is sensitive to high acidic media. The viscosity of guar in water depends on temperature, concentration, pH, shear rate. Guar shows shear thinning effect i.e. at high temperature it's solutions are less viscous but viscosity is regained when temperature is lowered.

Least Gel Residue

Information provided by Chemtotal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 6.5 - 8.0
@Time 1800 sec
6.5 - 8.0
@Time 0.500 hour
Brookfield Viscosity 9000 cP9000 cP
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 3.0 - 5.0 %3.0 - 5.0 %
 
Descriptive Properties
AppearanceOff White Powder
Sieve Test95%200 Mesh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for 7000 Series Aluminum Alloy
SABIC PVC 673E Emulsion Polyvinyl Chloride
Evonik TEGO® RHEO 8500 Thickener
Chemtotal F23 Guar Gum Powder
Chemours Teflon® PTFE Grade 304A Aqueous Dispersion

PCHEMT013 / 194954

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.