MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
CoorsTek AIN-170 Hot Pressed Aluminum Nitride  (discontinued **)
Categories: Ceramic; Nitride

Material Notes: Aluminum Nitride Advantages:
  • High heat dissipation with thermal conductivity of 170 W/m K
  • Non-toxic alternative to BeO
  • Thermal expansion coefficient similar to Si, GaN, and GaAs semiconductors
  • High dielectric strength

Information provided by CoorsTek, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.31 g/ccASTM C373
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength >= 350 MPaASTM F417
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm
@Temperature 25.0 °C
ASTM D257
Dielectric Constant 8.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength >= 15.0 kV/mm
@Thickness 0.635 mm
ASTM D149
Dissipation Factor 0.00020
Dielectric Loss Index 0.0016
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.20 µm/m-°C
@Temperature 25.0 - 1000 °C
ASTM C372
Thermal Conductivity >= 170 W/m-KASTM E1461
 
Descriptive Properties
Surface Finish As-fired (Ra) (micron)<0.5Profilometer 5.08µmicron Radius Stylus; 2,540 µmicron Cutoff ANSI/ASME B46.1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoorsTek Hot Pressed Aluminum Nitride
Aluminum Nitride, AlN
H.C. Starck Grade A Aluminum Nitride AIN
Indium Corp. Indalloy® 121 Sn-Ag Solder Alloy
CeramTec Alunit® Aluminum Nitride

CCOOR939 / 140554

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.