MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PolyMirae Moplen RP344RK Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen RP344RK is a nucleated polypropylene random copolymer manufactured by PolyMirae using Spheripol process technology licensed from LyondellBasell. Moplen RP344RK is specially designed for good processability and excellent clarity in low processing temperature with balanced mechanical properties. Moplen RP344RK is a random copolymer particularly suitable for injection molding of transparency container, houseware, thin walled articles for food and non food applications, stationery, caps and lids. Moplen RP344RK meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact.

Product Features: Good processability and excellent clarity in low processing temperature/High productivity with shorter cycle time than conventional random PP/Less bubbles(Voids) in final products/High gloss/Good mechanical property balance/Low odor and low taste transfer/Good color

Typical Applications: Transparency container, Houseware, Food container, TWIM, Stationery, Caps and lids, etc

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90ASTM D785
Tensile Strength, Yield 300 kg(f)/cm²ASTM D638
Elongation at Yield 8.0 %ASTM D638
Flexural Modulus 12500 kg(f)/cm²ASTM D790
Izod Impact, Notched 5.00 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 16 %ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyMirae Moplen RP5007K Injection Molding Grade Polypropylene
PolyMirae Moplen RP344N Injection Molding Grade Polypropylene
PolyMirae Moplen RP348NK Injection Molding Grade Polypropylene
PolyMirae Moplen RP5007 Injection Molding Grade Polypropylene
PolyMirae Moplen RP5058 Injection Molding Grade Polypropylene

PMIRAF54 / 183275

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.