MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyMirae Moplen RP5007 Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen RP5007 is a very high fluidity random copolymer. It is suitable for injection molding applications. The product is nucleated and contains anti static additive. Moplen RP5007 meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact. This is a developmental grade, changes in formulation and specification are possible. The information is valid at the time of writing. We suggest customers to check and confirm with us the most updated statements from time to time.

Product Features: Very high fluidity/ good transparency and gloss/ easy processing/ High Clarity/ resist dust pick up/ Low distortion

Typical Applications: DVD case/ Multi Media Packaging/ Containers/ Boxes / Houseware

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 75 g/10 min
@Load 2.16 kg,
Temperature 230 °C
75 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASMT D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9393ASTM D785
Tensile Strength, Yield 28.4 MPa4120 psiASTM D638
Elongation at Yield 10 %10 %ASTM D638
Flexural Modulus 1.18 GPa171 ksiASTM D790
Izod Impact, Notched  0.196 J/cm
@Temperature -20.0 °C
0.367 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 0.441 J/cm
@Temperature 23.0 °C
0.827 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen RP5007K Injection Molding Grade Polypropylene
PolyMirae Moplen RP5058 Injection Molding Grade Polypropylene
PolyMirae Moplen RP344RK Injection Molding Grade Polypropylene
PolyMirae Moplen RP344N Injection Molding Grade Polypropylene
PolyMirae Moplen RP348N Injection Molding Grade Polypropylene

PMIRAF59 / 183280

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.