MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

PolyMirae Moplen RP348N Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen RP348N is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP348N is a random copolymer particularly suitable for injection molding of houseware. Moplen RP348N meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact

Product Features: Excellent Transparency High gloss Good flowability Good impact rigidity balance/ Good surface finish and color/ Low odor and low taste transfer/ Improved injection molding cycle times

Typical Applications: Containers/ Housewares/ Bottles(ISBM)

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
11 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASMT D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.4 MPa4120 psiASTM D638
Elongation at Yield 13 %13 %ASTM D638
Flexural Modulus 1.05 GPa152 ksiASTM D790
Izod Impact, Notched 0.686 J/cm
@Temperature 23.0 °C
1.29 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C187 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen RP348NK Injection Molding Grade Polypropylene
PolyMirae Moplen RP344N Injection Molding Grade Polypropylene
PolyMirae Moplen RP348S Injection Molding Grade Polypropylene
PolyMirae Moplen RP5007K Injection Molding Grade Polypropylene
Lotte Advanced Materials Starex® VH-0800 ABS, Unreinforced FR

PMIRAF55 / 183276

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.