MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® R530H NT Nylon 66, 30% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Vydyne R530H NT is a general purpose, 30% glass-filled, heat-stabilized PA66 based resin designed for injection molding applications. R530H NT offers improved flow with a natural surface finish and maintains the excellent resistance typical of PA66 in chemicals, machine and motor oils, solvents, and gasoline.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³DAM; ISO 1183
Water Absorption 1.2 %
@Time 86400 sec
1.2 %
@Time 24.0 hour
DAM; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 2.00 mm
0.0050 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm
@Thickness 2.00 mm
0.012 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 135 MPa19600 psi50% RH; ISO 527-2
 195 MPa28300 psiDAM; ISO 527-2
Elongation at Break 3.0 %3.0 %DAM; ISO 527-2
 5.0 %5.0 %50% RH; ISO 527-2
Tensile Modulus 7.40 GPa1070 ksi50% RH; ISO 527-2
 10.0 GPa1450 ksiDAM; ISO 527-2
Flexural Strength 208 MPa30200 psi50% RH; ISO 178
 272 MPa39500 psiDAM; ISO 178
Flexural Modulus 8.10 GPa1170 ksi50% RH; ISO 178
 9.50 GPa1380 ksiDAM; ISO 178
Poissons Ratio 0.370.37ISO 527-2
Izod Impact, Notched (ISO)  11.0 kJ/m²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 11.0 kJ/m²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 11.0 kJ/m²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 13.0 kJ/m²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  6.10 J/cm²
@Temperature -40.0 °C
29.0 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eU
 6.30 J/cm²
@Temperature -30.0 °C
30.0 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 6.40 J/cm²
@Temperature -40.0 °C
30.5 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eU
 6.70 J/cm²
@Temperature -30.0 °C
31.9 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 7.20 J/cm²
@Temperature 23.0 °C
34.3 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 1.20 J/cm²
@Temperature -40.0 °C
5.71 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm
@Thickness 1.00 mm
1.00e+13 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
Dielectric Strength 20.0 kV/mm
@Thickness 1.00 mm
508 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
Arc Resistance 60 - 120 sec
@Thickness 3.00 mm
60 - 120 sec
@Thickness 0.118 in
PLC 6; ASTM D 495
Comparative Tracking Index 250 - 399 V
@Thickness 3.00 mm
250 - 399 V
@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 15 - 30 sec15 - 30 secPLC 3; UL 746
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min0.394 - 1.00 in/minPLC 1; UL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 22.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
12.2 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 76.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
42.2 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 260 °C500 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 261 °C502 °FUnannealed; 50% RH; ISO 75-2/B
 262 °C504 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FUnannealed; 50% RH; ISO 75-2/A
 252 °C486 °FUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical  140 °C
@Thickness 0.750 mm
284 °F
@Thickness 0.0295 in
UL 746
 140 °C
@Thickness 1.50 mm
284 °F
@Thickness 0.0591 in
UL 746
 140 °C
@Thickness 3.00 mm
284 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  120 °C
@Thickness 0.750 mm
248 °F
@Thickness 0.0295 in
UL 746
 120 °C
@Thickness 1.50 mm
248 °F
@Thickness 0.0591 in
UL 746
 120 °C
@Thickness 3.00 mm
248 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  125 °C
@Thickness 0.750 mm
257 °F
@Thickness 0.0295 in
UL 746
 140 °C
@Thickness 1.50 mm
284 °F
@Thickness 0.0591 in
UL 746
 140 °C
@Thickness 3.00 mm
284 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Flame Spread 0.000 mm/min
@Thickness 2.00 mm
0.000 in/min
@Thickness 0.0787 in
ISO 3795
Glow Wire Ignition Temperature  700 °C
@Thickness 0.750 mm
1290 °F
@Thickness 0.0295 in
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
1290 °F
@Thickness 0.0591 in
IEC 60695-2-13
 700 °C
@Thickness 3.00 mm
1290 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  675 °C
@Thickness 0.750 mm
1250 °F
@Thickness 0.0295 in
IEC 60695-2-12
 675 °C
@Thickness 1.50 mm
1250 °F
@Thickness 0.0591 in
IEC 60695-2-12
 675 °C
@Thickness 3.00 mm
1250 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Middle Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Front Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Nozzle Temperature 280 - 310 °C536 - 590 °FInjection
Melt Temperature 285 - 305 °C545 - 581 °FInjection
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D4066 PA012G30
 ASTM, D6779 PA012G30
 EC, 1935/2004
 EU, 10/2011
 EU, 2023/2006
 FDA, 21 CFR 177.1500
AppearanceNatural Color
Automotive Material SpecificationChery Q-SQR.S1-33-2012 CMP.PA66.G6
 Ford WSS-M4D752-B1
 GM GMW16270P-PA66-GF30
 GM GMW3038P-PA66-GF30H
 GM GMW3038P-PA66-GF30J
 HYUNDAI MS211-42 Type A
FeaturesAntifreeze Resistant
 Chemical Resistant
 Fatigue Resistant
 Gasoline Resistant
 Good Flow
 Heat Stabilized
 Lubricated
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Filled
DuPont Mobility and Materials Crastin® 6129 NC010 PBT
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon, 33% Glass Filled
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Filled

PASCE9803 / 220906

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.