System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Hexcel® HexPly® 920CX-EP2015-47.5% 125°C Curing Epoxy Matrix
Categories:
Polymer
;
Thermoset
;
Epoxy
;
Epoxy Cure Resin
Material Notes:
Intermediate modulus, 6K carbon, 2x2 twill, 193 g/m2
Information provided by HexCel
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
1337
MPa
pr EN 2561 Type B
Tensile Modulus
87.0
GPa
Results normalized to 60% fiber volume for Carbon, 50% fiber volume for Kevlar; pr EN 2561 Type B
Compressive Yield Strength
369
MPa
Compression After Impact @ 6.6 J/mm, Results normalized to 60% fiber volume for Carbon, 50% fiber volume for Kevlar; pr EN 6038
901
MPa
Results normalized to 60% fiber volume for Carbon, 50% fiber volume for Kevlar; EFA TP-003
Shear Strength
71.0
MPa
IL; pr EN 2563
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Solvay VTM® 260 series Epoxy Resin
Solvay MTM® 79 Epoxy Matrix with 50% CF1420 Carbon Fiber Composite
Overview of materials for Epoxy Cure Resin
Huntsman DY 9577 Epoxy Accelerator
E-Polymers SEPAZ® LA30 PA66 LFT Resin
PHEXC063 / 98533
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.