MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® 920CX-EP2015-47.5% 125°C Curing Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Intermediate modulus, 6K carbon, 2x2 twill, 193 g/m2

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 1337 MPa193900 psipr EN 2561 Type B
Tensile Modulus 87.0 GPa12600 ksiResults normalized to 60% fiber volume for Carbon, 50% fiber volume for Kevlar; pr EN 2561 Type B
Compressive Yield Strength 369 MPa53500 psiCompression After Impact @ 6.6 J/mm, Results normalized to 60% fiber volume for Carbon, 50% fiber volume for Kevlar; pr EN 6038
 901 MPa131000 psiResults normalized to 60% fiber volume for Carbon, 50% fiber volume for Kevlar; EFA TP-003
Shear Strength 71.0 MPa10300 psiIL; pr EN 2563

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay VTM® 260 series Epoxy Resin
Solvay MTM® 79 Epoxy Matrix with 50% CF1420 Carbon Fiber Composite
Overview of materials for Epoxy Cure Resin
Huntsman DY 9577 Epoxy Accelerator
E-Polymers SEPAZ® LA30 PA66 LFT Resin

PHEXC063 / 98533

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.