MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Chemlok® 402X-HS Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: LORD Chemlok® 402X-HS adhesive is a solvent-based, one-coat adhesive designed for bonding textiles to a wide variety of unvulcanized elastomers. Chemlok 402X-HS adhesive is an all-xylene version of Chemlok 402 adhesive. It is composed of a mixture of polymers, organic compounds and fillers dissolved or dispersed in an organic solvent system. Chemlok 402X-HS adhesive is used in the production of hoses, belts, diaphragms and other textile-reinforced rubber products. Chemlok 402X-HS adhesive can also be used as an additive to tie cements, primarily as a replacement for isocyanates that are widely used in rubber/textile bonding. A single coat of Chemlok 402X-HS adhesive will bond compounds based on a natural rubber (NR), polyisoprene (IR), styrene-butadiene (SBR), polybutadiene (BR), polychloroprene (CR), nitrile (NBR) and butyl (IIR) to polyester, polyamide, cotton, rayon, and polyaramid. When dried, Chemlok 402X-HS adhesive is tack-free.

Features: suitable for solvent incineration, saving cost of recovery equipment. bonds a variety of elastomers to a wide variety of textiles during vulcanization of the elastomer. adheres well to RFL-treated fabric or cord, giving excellent adhesion to these materials. Chemlok 402X-HS adhesive treated fabric or cord can be bonded immediately following solvent evaporation. requires only a single coat for most applications, reducing labor, solvent usage, inventory and shipping costs.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.65 - 8.10 lb/gal
Solids Content 23 - 26 %by weight
Brookfield Viscosity 600 - 1100 cP
@Temperature 25.0 °C
Brookfield LVT, Spindle 2, 30 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point 25.0 °CSeta
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 21.0 - 27.0 °C
from shipment date in original, unopened container. Moisture sensitive
 
Descriptive Properties
AppearanceBlack liquid
SolventsXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unitika AX-1500 Dry
Unitika AX-1500 Conditioned
Tra-Con Tra-Bond 2143D Medium Viscosity Polyamide Epoxy Adhesive
Lanxess Uniplex 214 Plastic Additive
Atom Adhesives AA-BOND FS227 Epoxy Adhesive

PLORD9027 / 232416

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.