MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Uniplex 214 Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex 214 is a liquid sulfonamide compatible with a number of resins but is mainly used as plasticizer for polyamides especially PA 11, PA 12 and copolyamides.

Chemical composition: N-Butylbenzenesulfonamide (N-BSA)

General Uniplex 214 is a liquid sulfonamide plasticizer compatible with a number of resins, such as polyacetals, polyacrylates, polycarbonates, polysulfones, cellulose derivatives, and polyamides. Uniplex 214 is especially used as plasticizer for PA 11 and PA 12. It is also compatible with PA 6, PA 6.6 and copolyamides.

Applications: Uniplex 214 is the preferred primary plasticizer for polyamide resins, greatly enhancing low temperature flexibility. Uniplex 214 may be added either pre- or post-polymerization for PA 11 or PA 12, or in the extrusion of other polyamides (e.g. PA 6, PA 6.6). It is typically used at levels of 5 - 20%, based on the weight of the polymer. The addition of this plasticizer contributes the following properties:

  • Easier removal from molds
  • Easier machining
  • Better finish
  • Good heat stability to 80°C
  • Better shape stability due to reduced water absorption
Uniplex 214 is used in such applications as molded polyamide parts, nylon filaments, e.g. fishing and grass trimmer lines, nylon-based hot melt adhesives and adhesives for nonwoven interlinings, fuel lines, hoses, films and other high performance applications.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.149 g/cc0.04151 lb/in³Relative
pH 7.5 - 8.57.5 - 8.5
Brookfield Viscosity 165 cP165 cPdynamic
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5241.524
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %Karl Fischer
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Appearanceclear liquid
Color<250Hazen, 3 hrs at 250°C
 <50Hazen
Content<50 mg/kgInorganic Chloride
Specifications<4 mEq/kgBasicity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Global EPP POM C Acetal Copolymer
Hippe POM Copolymer
SEKISUI SPI KYDEX® V103 Thermoplastic
Sandvik 13C26 razor blade steel Strip
Rogers Arlon AD250 Woven Glass and PTFE

PLANY9103 / 209494

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.