MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petropol Triapol® F3 K55 PRTA010 BS311 PC/PBT
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Product Description: Polybutadiene Terephthalate / Polycarbonate Blend

Resin ID (ISO 1043): PBT+PC
Processing: Injection Molding
Color: Black

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 - 1.22 g/cc0.0426 - 0.0441 lb/in³ASTM D792
Water Absorption 0.080 - 0.13 %0.080 - 0.13 %Equilibrium; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.021 cm/cm
@Thickness 3.20 mm
0.0050 - 0.021 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 90 g/10 min
@Load 5.00 kg,
Temperature 270 °C
90 g/10 min
@Load 11.0 lb,
Temperature 518 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 54.0 MPa7830 psiASTM D638
Elongation at Break 150 %150 %ASTM D638
Flexural Strength 80.0 MPa11600 psiASTM D790
Flexural Modulus 1.90 GPa276 ksiASTM D790
Izod Impact, Notched >= 6.00 J/cm>= 11.2 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C219 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C180 °FASTM D648
Vicat Softening Point  118 °C
@Load 5.10 kg
244 °F
@Load 11.2 lb
120 °C/h; ASTM D1525
 153 °C
@Load 5.10 kg
307 °F
@Load 11.2 lb
50 °C/h; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 - 280 °C482 - 536 °FMolding
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 100 °C212 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL425 / 313333

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.