System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Petropol Triapol® F3 K55 PRTA010 BS311 PC/PBT
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Material Notes:
Product Description: Polybutadiene Terephthalate / Polycarbonate Blend
Resin ID (ISO 1043): PBT+PC
Processing: Injection Molding
Color: Black
Information provided by Petropol
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.18
-
1.22
g/cc
ASTM D792
Water Absorption
0.080 - 0.13 %
Equilibrium; ASTM D570
Linear Mold Shrinkage, Flow
0.0050
-
0.021
cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow
90
g/10 min
@Load 5.00 kg,
Temperature 270 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength
54.0
MPa
ASTM D638
Elongation at Break
150 %
ASTM D638
Flexural Strength
80.0
MPa
ASTM D790
Flexural Modulus
1900
MPa
ASTM D790
Izod Impact, Notched
>=
600
J/m
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
104
°C
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
82.0
°C
ASTM D648
Vicat Softening Point
118
°C
@Load 5.10 kg
120 °C/h; ASTM D1525
153
°C
@Load 5.10 kg
50 °C/h; ASTM D1525
Processing Properties
Original Value
Comments
Processing Temperature
250
-
280
°C
Molding
Mold Temperature
80.0
-
100
°C
Drying Temperature
100
°C
Dry Time
4.00
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PPETROPOL425 / 313333
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.