MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ZEON Zetpol® 2000 Hydrogenated Nitrile Elastomomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Zeptol 2000 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, excellent heat resistance, good checmial resistance to aggressive fluids, and an excellent balance of perperties over a wide variation of temperatures.

For O-rings, gaskets, seals, or oil field components requiring the best heat and ozone resistance. FDA approved.

Key Words: HNBR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/cc
Iodine Absorption Number <= 7.0mg/100mg; ZCI-T-004
Mooney Viscosity 78 - 92
@Temperature 100 °C
(1+4); ZCI-T-003
Ash <= 0.50 %ZCI-T-005
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A >= 62ZCI-T-009
Tensile Strength at Break >= 2828 psiZCI-T-008
Elongation at Break >= 350 %ZCI-T-008
300% Modulus >= 1.276 ksi
@Strain 300 %
ZCI-T-008
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
% HYD>99.5
Bound ACN (%, acrylonitrile)34.9-37.5
Heat Loss (%) Max0.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ZEON Zetpol® 2010L Hydrogenated Nitrile Elastomomer
ZEON Zetpol® PBZ-123 Hydrogenated Nitrile Elastomomer
Freudenberg S60 Silicone Elastomer (VMQ)
Hydrogenated Nitrile Rubber (HNBR)
Klinger Thermoseal Klinger® Quantum Hydrogenated Nitrile Butadiene Rubber (HNBR)

PZEONC04 / 73063

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.