MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Freudenberg S60 Silicone Elastomer (VMQ)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasoline and solvents; poor resistance to alkalis and acids.

This product was formerly sold under the Freudenberg Simrit division; now Freudenberg Sealing Technologies.

Key Words: BAYSOLINE®, SILASTIC® , SILPLUS®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060Original Property; ASTM D2240
 5353ASTM #1 Oil Immersion for 70 hours; ASTM D2240
 6666Air Aging, 70 hours; ASTM D2240
Tensile Strength, Ultimate 6.60 MPa957 psiOriginal Property; ASTM D412 Die C
 5.830 MPa845.5 psiAir Aging, 70 hours; ASTM D412 Die C
 6.03 MPa874 psiASTM #1 Oil Immersion for 70 hours; ASTM D412 Die C
Elongation at Break 350 %350 %Original Property; ASTM D412 Die C
 248.5 %248.5 %Air Aging, 70 hours; ASTM D412 Die C
 322 %322 %ASTM #1 Oil Immersion for 70 hours; ASTM D412 Die C
Tear Strength 17.9 kN/m102 pliASTM D624 Die B
Compression Set  19 %
@Temperature 150 °C,
Time 252000 sec
19 %
@Temperature 302 °F,
Time 70.0 hour
25 max; ASTM D395
 19 %
@Temperature 150 °C,
Time 252000 sec
19 %
@Temperature 302 °F,
Time 70.0 hour
40 max; ASTM D395
 19 %
@Temperature 150 °C,
Time 252000 sec
19 %
@Temperature 302 °F,
Time 70.0 hour
ASTM D395 Method B
 
Descriptive Properties
Bend (flat)PassAir Aging for 70 hours at 225°C
ColorRed
Decomposition per AMS 3302GNone
Low Temperature BrittlenessPass, No cracksASTM D2137
Surface Tackiness per AMS 3302GNone
Volume Change (%), ASTM D4712Water Immersion for 70 hours at 100°C
 6ASTM #1 Oil Immersion for 70 hours at 150°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Freudenberg S40 Silicone Elastomer (VMQ)
Freudenberg S50 Silicone Elastomer (VMQ)
Freudenberg S70 Silicone Elastomer (VMQ)
Freudenberg S315 Silicone Elastomer (VMQ)
Freudenberg S313 Silicone Elastomer (VMQ)

PSIMR146 / 79108

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.