MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestodur® X7347 nf PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: Flame resistant, medium viscosity, impact resistant PBT-Resin with higher tracking reference number for injection molding.

Applications: Electrical and electronics industries.

ISO data as provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/cc
Water Absorption 0.00 %
Melt Flow 50 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 40.0 MPa
Elongation at Break 30 %
Elongation at Yield 3.0 %
Modulus of Elasticity 2.20 GPa
Charpy Impact Unnotched NB
 20.0 J/cm²
@Temperature -30.0 °C
Charpy Impact, Notched 1.40 J/cm²
 0.800 J/cm²
@Temperature -30.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cm
Surface Resistance 1.00e+13 ohm
Dielectric Constant 3.0
@Frequency 100 Hz
 3.0
@Frequency 1e+6 Hz
Dielectric Strength 25.0 kV/mm
Dissipation Factor 0.0075
@Frequency 100 Hz
 0.025
@Frequency 1e+6 Hz
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 20.0 °C
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 170 °C
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
Vicat Softening Point 175 °C50°C/hr/50 N
Flammability, UL94 V-0
@Thickness 1.60 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestodur® 1003-FR5 Flame Retardant PBT
Evonik Vestodur® X7061 Laser Markable PBT
Evonik Vestodur® HI19-FR2 nf PBT
Evonik Vestodur® 2002-FR3 Laser Markable PBT
Celanese Celanex® 1400A PBT, Unfilled

PHUM38 / 47471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.