MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestodur® 2002-FR3 Laser Markable PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Description: Degussa AG’s High Performance Polymers Business Unit manufactures a range of polybutylene terephthalate compounds that are supplied under the registered trademark VESTODUR® . Material properties characterizing VESTODUR compounds are:
  • high thermostability
  • high stiffness
  • low water absorption resulting in high dimensional stability
  • high hardness
  • good strength
  • good sliding friction behavior, low abrasion
  • good creep behavior
  • good electrical properties
  • good chemical resistance
  • good weathering resistance
  • good processability
  • no tendency to form stress cracks

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PBT-FR-MV
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 3.10 GPa450 ksi
Izod Impact, Notched (ISO) 50.0 kJ/m²23.8 ft-lb/in²180/1C
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 180 °C356 °F
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Descriptive Properties
ColorNatural

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestodur® X7347 nf PBT
Evonik Vestodur® X7061 Laser Markable PBT
Evonik Vestodur® GF 20 20% Glass Reinforced PBT
BASF Ultradur® FRee B 4450 G5 LS 25% Glass Filled PBT
Evonik Vestoran® X7342 20% Glass Reinforced Laser Markable PPE Compound

PHUMA05 / 47519

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.