MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
E-Polymers TEKASTER® F101M Unreinforced impact modified PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Impact Grade

Material Notes: Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical performance. Specially G/F reinforced PET has excellent heat resistance, a good surface, chemical resistance and high electrical performance.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D792
Linear Mold Shrinkage 0.016 cm/cm
Linear Mold Shrinkage, Transverse 0.030 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 49.05 MPaASTM D638
Elongation at Break >= 120 %ASTM D638
Flexural Strength 70.63 MPaASTM D790
Flexural Modulus 1863.9 MPaASTM D790
Izod Impact, Notched 5.00 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 153 °CASTM D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 250 °C
Mold Temperature 40.0 - 60.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
E-Polymers Tekaloy® T80 , Dimensional Stability PBT/ABS Alloy
E-Polymers Tekaloy® T80HI Impact Resistance PBT/ABS Alloy
E-Polymers Tekaloy® T80G20 , 20% Glass Fiber Reinforced PBT/ABS Alloy
Epsan Epimix PBT-PET GV0 30 NC Q1D001 Polybutylene Terephthalate/Polyethylene terephthalate
Epsan Epimix PBT/PET GFR 30 NC Polybutylene Terephthalate/Polyethylene terephthalate

PEPOLZ024 / 103521

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.