MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epsan Epimix PBT-PET GV0 30 NC Q1D001 Polybutylene Terephthalate/Polyethylene terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: Flame retardant, reinforced with 30% of glass fiber, heat stabilized, lubricated for injection molding. Used in all sectors of industry, compliance with RoHs derivatives, with rating UL94 V0, offering a perfect balance of thermal and mechanical properties.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.72 g/cc0.0621 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inParallel; ISO 294-4
 0.010 cm/cm0.010 in/inNormal; ISO 294-4
Ash 30 %30 %ISO 3451-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 135 MPa19600 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Tensile Modulus 11.5 GPa1670 ksiISO 527-2
Flexural Strength 195 MPa28300 psiISO 178
Flexural Modulus 9.75 GPa1410 ksiISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 250 V250 VEN 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
EN 60695-11-10
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FRecommended Injection Molding Temperature
Drying Temperature 80.0 °C176 °FAverage Drying Time is 2-4 hrs
Moisture Content 0.20 %0.20 %ISO 15512

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Polymers Tekaloy® T80HI Impact Resistance PBT/ABS Alloy
E-Polymers TEKASTER® F101M Unreinforced impact modified PBT
Epsan Epimix PBT/PET GFR 30 NC Polybutylene Terephthalate/Polyethylene terephthalate
Celanese Crastin® SK642FR BK851 Polybutylene Terephthalate (PBT)
Celanese Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)

PEPSAN002 / 186316

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.