Lustran® 556 resin is a low-gloss, medium-impact extrusion grade of ABS (acrylonitrile butadiene styrene). It has good melt strength for extrusion and thermoforming, and can be easily coextruded. Features: Low gloss, Medium impact strength, Ease of coloring, UL 94 HB rated. Applications: Motor vehicle dashboards, Interior panels, Interior trim.Information provided by Styrolution. |