MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

INEOS Styrolution Lustran® 556 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Lustran® 556 resin is a low-gloss, medium-impact extrusion grade of ABS (acrylonitrile butadiene styrene). It has good melt strength for extrusion and thermoforming, and can be easily coextruded. Features: Low gloss, Medium impact strength, Ease of coloring, UL 94 HB rated. Applications: Motor vehicle dashboards, Interior panels, Interior trim.

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 22.1 MPa3210 psiASTM D 638
Tensile Strength, Yield 19.3 MPa2800 psiASTM D 638
Tensile Modulus 1.52 GPa220 ksiASTM D 638
Flexural Yield Strength 31.0 MPa
@Strain 5.0 %
4500 psi
@Strain 5.0 %
ASTM D 790
Flexural Modulus 1.45 GPa210 ksiASTM D 790
Izod Impact, Notched  0.534 J/cm
@Temperature -40.0 °C
1.00 ft-lb/in
@Temperature -40.0 °F
ASTM 256
 0.694 J/cm
@Temperature -18.0 °C
1.30 ft-lb/in
@Temperature -0.400 °F
ASTM 256
 1.07 J/cm
@Temperature 23.0 °C
2.00 ft-lb/in
@Temperature 73.4 °F
ASTM 256
Dart Drop, Total Energy 25.8 J19.0 ft-lbPeak force; ASTM D 3763
 29.8 J22.0 ft-lbTotal energy; ASTM D 3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 97.2 µm/m-°C54.0 µin/in-°FASTM D 696
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C205 °Funannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °Funannealed; ASTM D 648
 
Optical PropertiesMetricEnglishComments
Gloss <= 10 %<= 10 %at 60°, specular; ASTM D 523
 
Processing PropertiesMetricEnglishComments
Drying Temperature 79.0 °C
@Time 7200 - 14400 sec
174 °F
@Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Lustran® 235 Acrylonitrile Butadiene Styrene (ABS)
INEOS Styrolution Lustran® 1152 Acrylonitrile Butadiene Styrene (ABS)
INEOS Styrolution Lustran® 752 Acrylonitrile Butadiene Styrene (ABS)
INEOS Styrolution Lustran® 732 Acrylonitrile Butadiene Styrene (ABS)
INEOS Styrolution Lustran® 682 Acrylonitrile Butadiene Styrene (ABS)

PSTYR9889 / 216116

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.