MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper, UNS C18100, Cold Worked (60% reduction) Wire
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent capacity for both cold and hot forming. Excellent solderability. Good brazing and gas-shielded arc welding. Fair butt resistance welding.

Applications: resistance welding electrodes and wheels, switches, circuit breakers, high temperature wire, semiconductor bases, heat sinks, and continuous casting molds.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.88 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 480 MPa
Tensile Strength, Yield 435 MPa
Elongation at Break 6.0 %in 50 mm
Modulus of Elasticity 125 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000217 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.7 µm/m-°C
@Temperature 20.0 - 100 °C
 20.4 µm/m-°C
@Temperature 20.0 - 200 °C
 21.3 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0940 BTU/lb-°F
Thermal Conductivity 324 W/m-K
Melting Point <= 1075 °C
Liquidus 1075 °C
Annealing Point 1100 - 1300 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 600 - 700 °C
Solution Temperature 900 - 975 °CFor 1 hour
Aging Temperature 400 - 500 °CFor 1 hour
Hot-Working Temperature 790 - 925 °C
Precipitation Temperature >= 840 °FAir
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 0.40 - 1.2 %
Copper, Cu 99 %
Magnesium, Mg 0.030 - 0.060 %
Zirconium, Zr 0.050 - 0.30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper
MetalTek C18100 Chrome Zirc Copper High Conductivity
Ampco Metal AMPCOLOY® 972 Chromium-Copper Alloy, Extruded and Drawn Rods, 50 - 120 mm.
Ampco Metal AMPCOLOY® 972 Chromium-Copper Alloy, Extruded and Drawn Rods, 10 - 25 mm.
Cadi 1815 Copper Alloy

MC18100b3 / 10907

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.