MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ampco Metal AMPCOLOY® 972 Chromium-Copper Alloy, Extruded and Drawn Rods, 50 - 120 mm.
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: AMPCOLOY 972 is a precipitation hardening copper-base-alloy. In the heat treated condition, this alloy retains the mechanical properties together with a good ductility in the range of 300-500°C. High electrical conductivity and high mechanical properties are attributes of this versatile alloy.

Applications: Resistance welding tips; Electrode caps for the automotive industry; Tong arms for welding robots; Electrode holders; Parts for energy engineering; Press parts

Key Words: CDA C18150; CDA C18200; CDA C18400; RWMA Class2, CuCr1Zr; EN CW 106C; DIN 44759 A 2/2 17666 W.Nr. 2.1293; AFNOR UC1Zr
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 125125HB 10
Hardness, Rockwell B 7272
Tensile Strength, Ultimate 465 MPa67400 psi
Tensile Strength, Yield 410 MPa
@Strain 0.5 %
59500 psi
@Strain 0.5 %
Elongation at Break 18 %18 %
Modulus of Elasticity 120 GPa17400 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000196 ohm-cm0.00000196 ohm-cm86% I.A.C.S.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 °C
9.44 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 320 W/m-K2220 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 1.0 %1.0 %
Copper, Cu 98.7 - 98.9 %98.7 - 98.9 %As Balance
Other, total <= 0.20 %<= 0.20 %
Zirconium, Zr 0.10 %0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper
Ampco Metal AMPCOLOY® 972 Chromium-Copper Alloy, Extruded and Drawn Rods, 10 - 25 mm.
Ampco Metal AMPCOLOY® 972 Chromium-Copper Alloy, Extruded and Drawn Rods, 25 - 50 mm.
Cadi 1815 Copper Alloy
Ampco Metal AMPCOLOY® 95 Cobalt-Copper Alloy, Extrusion, >50.8 mm.

NAMPCO48 / 15002

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.