MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ineos Styrenics Avantra® 2710 High Impact Styrenic Polymer (Global)  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Description: Avantra® 2710 is a high-impact grade of polystyrene with improved stress crack resistance, developed primarily for extrusion and thermoforming applications, especially for the refrigerator industry.

Information provided by BASF.


Ineos Styrenics purchased this product line from BASF in 2005.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Moisture Absorption at Equilibrium <= 0.10 %<= 0.10 %23°C/50% RH
Water Absorption at Saturation <= 0.10 %<= 0.10 %
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 2.6 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.6 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 4242ASTM D785
Tensile Strength at Break 23.0 MPa3340 psiASTM D638
Tensile Strength, Yield 17.0 MPa2470 psiASTM D638
Elongation at Break 65 %65 %ASTM D638
Tensile Modulus 1.655 GPa240.0 ksiASTM D638
Flexural Modulus 1.38 GPa200 ksiASTM D790-1
Izod Impact, Notched 1.23 J/cm2.30 ft-lb/inASTM D256-A
Gardner Impact 20.3 J
@Thickness 3.17 mm,
Temperature 23.0 °C
15.0 ft-lb
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D3029
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.30e+13 ohm-cm1.30e+13 ohm-cmASTM D257
Dielectric Strength 44.4 kV/mm1130 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FASTM D648
Vicat Softening Point 101 °C214 °FASTM D1525
Flammability, UL94  HB
@Thickness 1.10 mm
HB
@Thickness 0.0433 in
White
 HB
@Thickness 1.47 mm
HB
@Thickness 0.0579 in
CSA 0.6 Natural
 
Optical PropertiesMetricEnglishComments
Gloss 10 %10 %60°; ASTM D523
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 230 °C392 - 446 °FExtrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos Styrenics Avantra® 585K Rubber Modified Polystyrene
Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene
Greene Tweed Avalon® 11 PTFE, Carbon, Graphite Filled
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA)
Ineos Styrenics Avantra® 594E High Impact Styrenic Polymer (NAFTA)

PSG107 / 67268

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.