MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Tin Alloy
Categories: Metal; Nonferrous Metal; Tin Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Tin Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.76 - 9.66 g/cc0.208 - 0.349 lb/in³Average value: 7.80 g/cc Grade Count:188
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 3.90 - 40.03.90 - 40.0Average value: 16.4 Grade Count:44
Hardness, Vickers 12.9 - 16.112.9 - 16.1Average value: 15.4 Grade Count:4
Tensile Strength, Ultimate 9.65 - 448 MPa1400 - 65000 psiAverage value: 59.3 MPa Grade Count:101
Tensile Strength, Yield 11.0 - 43.0 MPa1600 - 6240 psiAverage value: 33.0 MPa Grade Count:5
Elongation at Break 1.00 - 136 %1.00 - 136 %Average value: 39.2 % Grade Count:53
Modulus of Elasticity 14.5 - 53.0 GPa2110 - 7690 ksiAverage value: 37.4 GPa Grade Count:39
Compressive Yield Strength 30.3 - 121 MPa4390 - 17600 psiAverage value: 69.5 MPa Grade Count:7
Poissons Ratio 0.330 - 0.4000.330 - 0.400Average value: 0.381 Grade Count:7
Fatigue Strength 20.6 - 33.0 MPa2990 - 4790 psiAverage value: 25.0 MPa Grade Count:4
Shear Modulus 11.0 - 15.6 GPa1600 - 2260 ksiAverage value: 12.1 GPa Grade Count:7
Shear Strength 11.2 - 76.5 MPa1620 - 11100 psiAverage value: 39.7 MPa Grade Count:26
Izod Impact 3.40 - 27.1 J2.51 - 20.0 ft-lbAverage value: 18.9 J Grade Count:14
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000104 - 0.0000340 ohm-cm0.0000104 - 0.0000340 ohm-cmAverage value: 0.0000151 ohm-cm Grade Count:70
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 - 36.0 µm/m-°C7.78 - 20.0 µin/in-°FAverage value: 24.0 µm/m-°C Grade Count:71
Specific Heat Capacity 0.167 - 0.272 J/g-°C0.0399 - 0.0650 BTU/lb-°FAverage value: 0.211 J/g-°C Grade Count:16
Thermal Conductivity 20.7 - 73.0 W/m-K144 - 507 BTU-in/hr-ft²-°FAverage value: 48.0 W/m-K Grade Count:46
Melting Point 93.0 - 422 °C199 - 792 °FAverage value: 203 °C Grade Count:192
Solidus 93.0 - 250 °C199 - 482 °FAverage value: 189 °C Grade Count:171
Liquidus 93.0 - 422 °C199 - 792 °FAverage value: 214 °C Grade Count:166
Boiling Point 2600 °C4720 °FAverage value: 2600 °C Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 221 - 450 °C430 - 842 °FAverage value: 256 °C Grade Count:6
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.00100 - 0.0300 %0.00100 - 0.0300 %Average value: 0.00588 % Grade Count:34
Antimony, Sb 0.00800 - 16.0 %0.00800 - 16.0 %Average value: 3.91 % Grade Count:70
Arsenic, As 0.000500 - 2.00 %0.000500 - 2.00 %Average value: 0.0991 % Grade Count:44
Bismuth, Bi 0.00100 - 46.0 %0.00100 - 46.0 %Average value: 6.48 % Grade Count:53
Cadmium, Cd 0.00100 - 32.2 %0.00100 - 32.2 %Average value: 5.04 % Grade Count:34
Copper, Cu 0.00200 - 8.50 %0.00200 - 8.50 %Average value: 1.53 % Grade Count:77
Germanium, Ge 0.0100 - 1.00 %0.0100 - 1.00 %Average value: 0.208 % Grade Count:5
Indium, In 0.0500 - 52.2 %0.0500 - 52.2 %Average value: 23.5 % Grade Count:26
Iron, Fe 0.00400 - 0.0800 %0.00400 - 0.0800 %Average value: 0.0370 % Grade Count:42
Lead, Pb 0.0100 - 70.0 %0.0100 - 70.0 %Average value: 24.8 % Grade Count:119
Nickel, Ni 0.00500 - 0.0500 %0.00500 - 0.0500 %Average value: 0.0352 % Grade Count:6
Silver, Ag 0.00200 - 25.0 %0.00200 - 25.0 %Average value: 3.26 % Grade Count:65
Sulfur, S 0.00200 - 0.0100 %0.00200 - 0.0100 %Average value: 0.00625 % Grade Count:4
Tin, Sn 30.0 - 100 %30.0 - 100 %Average value: 77.9 % Grade Count:216
Zinc, Zn 0.00100 - 34.0 %0.00100 - 34.0 %Average value: 2.00 % Grade Count:50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tin, Sn
Silver Tin Selenide, AgSnSe3
Lead-Tin Babbitt Alloy
Overview of materials for Lead Alloy
Overview of materials for Silver Alloy

M01069 / 81678

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.