MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Lead Alloy
Categories: Metal; Nonferrous Metal; Lead Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Lead Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.15 - 11.7 g/cc0.294 - 0.422 lb/in³Average value: 10.5 g/cc Grade Count:422
Thickness 102 - 173 microns4.00 - 6.80 milAverage value: 141 microns Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 3.00 - 33.03.00 - 33.0Average value: 11.8 Grade Count:64
Tensile Strength, Ultimate 12.0 - 1520 MPa1740 - 220000 psiAverage value: 95.2 MPa Grade Count:139
Tensile Strength, Yield 6.00 - 1130 MPa870 - 164000 psiAverage value: 368 MPa Grade Count:12
Elongation at Break 2.00 - 101 %2.00 - 101 %Average value: 32.5 % Grade Count:81
Modulus of Elasticity 13.8 - 215 GPa2000 - 31200 ksiAverage value: 27.9 GPa Grade Count:33
Poissons Ratio 0.380 - 0.4200.380 - 0.420Average value: 0.400 Grade Count:3
Shear Modulus 4.90 - 12.0 GPa711 - 1740 ksiAverage value: 9.30 GPa Grade Count:3
Shear Strength 12.4 - 52.0 MPa1800 - 7540 psiAverage value: 26.3 MPa Grade Count:22
Adhesive Bond Strength 19.5 - 30.0 MPa2830 - 4350 psiAverage value: 23.6 MPa Grade Count:5
Peel Strength 0.340 - 0.548 kN/m1.94 - 3.13 pliAverage value: 0.455 kN/m Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000140 - 0.0000430 ohm-cm0.0000140 - 0.0000430 ohm-cmAverage value: 0.0000242 ohm-cm Grade Count:86
Magnetic Susceptibility -1.20e-7-1.20e-7Average value: -1.20e-7 Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.8 - 30.4 µm/m-°C6.55 - 16.9 µin/in-°FAverage value: 25.4 µm/m-°C Grade Count:105
Specific Heat Capacity 0.100 - 0.197 J/g-°C0.0240 - 0.0471 BTU/lb-°FAverage value: 0.136 J/g-°C Grade Count:30
Thermal Conductivity 15.0 - 58.0 W/m-K104 - 403 BTU-in/hr-ft²-°FAverage value: 33.0 W/m-K Grade Count:77
Melting Point 47.0 - 579 °C117 - 1070 °FAverage value: 238 °C Grade Count:187
Solidus 47.0 - 327 °C117 - 621 °FAverage value: 218 °C Grade Count:171
Liquidus 47.0 - 579 °C117 - 1070 °FAverage value: 251 °C Grade Count:170
Boiling Point 1750 °C3180 °FAverage value: 1750 °C Grade Count:7
Maximum Service Temperature, Air 82.0 - 121 °C180 - 250 °FAverage value: 104 °C Grade Count:4
Minimum Service Temperature, Air -51.0 - -18.0 °C-59.8 - -0.400 °FAverage value: -38.5 °C Grade Count:4
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.6300.630Average value: 0.630 Grade Count:3
Reflection Coefficient, Visible (0-1) 0.6200.620Average value: 0.620 Grade Count:4
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.00100 - 1.90 %0.00100 - 1.90 %Average value: 0.0492 % Grade Count:67
Antimony, Sb 0.000500 - 29.0 %0.000500 - 29.0 %Average value: 5.07 % Grade Count:207
Arsenic, As 0.000500 - 3.00 %0.000500 - 3.00 %Average value: 0.264 % Grade Count:93
As + Sb + Sn 0.00200 %0.00200 %Average value: 0.00200 % Grade Count:6
Barium, Ba 0.0500 - 2.00 %0.0500 - 2.00 %Average value: 0.491 % Grade Count:11
Bismuth, Bi 0.00500 - 55.5 %0.00500 - 55.5 %Average value: 6.67 % Grade Count:102
Boron, B 0.0100 %0.0100 %Average value: 0.0100 % Grade Count:3
Cadmium, Cd 0.000500 - 17.0 %0.000500 - 17.0 %Average value: 1.03 % Grade Count:37
Calcium, Ca 0.00800 - 6.00 %0.00800 - 6.00 %Average value: 0.376 % Grade Count:41
Carbon, C 0.100 - 0.150 %0.100 - 0.150 %Average value: 0.117 % Grade Count:3
Chromium, Cr 20.5 - 23.0 %20.5 - 23.0 %Average value: 22.0 % Grade Count:3
Cobalt, Co 0.500 - 19.0 %0.500 - 19.0 %Average value: 7.33 % Grade Count:3
Copper, Cu 0.000500 - 55.0 %0.000500 - 55.0 %Average value: 1.19 % Grade Count:94
Indium, In 1.00 - 60.0 %1.00 - 60.0 %Average value: 21.1 % Grade Count:40
Iron, Fe 0.000500 - 20.0 %0.000500 - 20.0 %Average value: 0.560 % Grade Count:70
Lead, Pb 22.6 - 100 %22.6 - 100 %Average value: 81.7 % Grade Count:448
Lithium, Li 0.0100 - 0.700 %0.0100 - 0.700 %Average value: 0.151 % Grade Count:14
Nickel, Ni 0.000500 - 53.8 %0.000500 - 53.8 %Average value: 20.3 % Grade Count:7
Selenium, Se 0.00500 - 0.0200 %0.00500 - 0.0200 %Average value: 0.0140 % Grade Count:5
Silver, Ag 0.000100 - 40.0 %0.000100 - 40.0 %Average value: 2.32 % Grade Count:90
Strontium, Sr 0.0600 - 2.00 %0.0600 - 2.00 %Average value: 0.605 % Grade Count:4
Sulfur, S 0.00100 - 0.500 %0.00100 - 0.500 %Average value: 0.0353 % Grade Count:18
Tellurium, Te 0.0350 - 0.0600 %0.0350 - 0.0600 %Average value: 0.0419 % Grade Count:4
Tin, Sn 0.000500 - 63.0 %0.000500 - 63.0 %Average value: 17.3 % Grade Count:304
Titanium, Ti 0.150 - 3.70 %0.150 - 3.70 %Average value: 1.33 % Grade Count:3
Tungsten, W 0.200 - 2.00 %0.200 - 2.00 %Average value: 1.07 % Grade Count:3
Zinc, Zn 0.000500 - 0.0100 %0.000500 - 0.0100 %Average value: 0.00463 % Grade Count:72

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nickel Alloy
Overview of materials for Copper Alloy
Overview of materials for Molybdenum Alloy
Overview of materials for Tin Alloy
Lead, Pb

M01058 / 81671

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.