MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay SIPOMER® WAM II Composition Based On Methacrylamidoethyl Ethylene Urea
Categories: Fluid

Material Notes: Description: Specialty monomer for Wet Adhesion Promotion

Identification: COMPOSITION BASED ON METHACRYLAMIDOETHYL ETHYLENE UREA

CAS: 3089 – 19 – 8

Solubility: Total in water

Polymer Test (10% in methanol): Limpid to slightly hazy, AN4021

Inhibitor: HA/1800

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Co-monomer in latex manufacturing. Improve the wet adhesion effect.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/cc
Volatiles <= 57 %
pH 2.0 - 5.010% aq. Sol.; AN3401
Viscosity 20 cP
Molecular Weight 197 g/mol
 
Thermal PropertiesOriginal ValueComments
Crystallization Temperature -15.0 °C
Boiling Point 100 °C
Glass Transition Temp, Tg 87.0 °C
Flash Point >= 100 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content 24.5 - 28.5 %AN3150
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceThick liquid
CompositionAEEU<3%, AN3372
 Hydroquinone0.15-0.25%, AN7013
 MAEEU46-50%, AN7045
 Methacrylic acid22.5-26%, AN3371

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay SIPOMER® WAM Allyl / Ureido Monomer
Solvay SIPOMER® SEM 25 Polyalkoxyl Polyarylphenol Ethylenic Methacrylate
Solvay SIPOMER® PAM-4000 Ethylmethacrylate Phosphate; Alkyl Methacrylate Phosphate
Solvay SIPOMER® PAM-300 Phosphate Esters of Ppg Monoacrylate
Solvay SIPOMER® PAM-100 Phosphate Esters of Polyethylene Glycol Monomethacrylate

WRHOD510 / 137741

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.