MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay SIPOMER® WAM Allyl / Ureido Monomer
Categories: Fluid

Material Notes: Description: Specialty monomer for Wet Adhesion Promotion

Identification: ALLYL / UREIDO MONOMER

CAS: 90412 – 00 – 3

EINECS: 291 – 480 – 2

Solubility: Soluble in water. Insoluble in most organic solvents.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Adhésives. Paints.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
Solids Content 89 - 91 %89 - 91 %100% water; AN3150
Viscosity 500 cP500 cP
Molecular Weight 357 g/mol357 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point -10.0 °C14.0 °FFreezing Point
Flash Point 110 °C230 °FClosed cup
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 10<= 10AN3013
 
Processing PropertiesMetricEnglishComments
Moisture Content 9.0 - 11 %9.0 - 11 %AN3150
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceClear amber liquid
CompositionActive0.9
 Total amine2.3-2.7 MEQ/g
 Unsaturation9.5-10.8 MEQ/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay SIPOMER® WAM II Composition Based On Methacrylamidoethyl Ethylene Urea
Solvay SIPOMER® SEM 25 Polyalkoxyl Polyarylphenol Ethylenic Methacrylate
Solvay SIPOMER® PAM-4000 Ethylmethacrylate Phosphate; Alkyl Methacrylate Phosphate
Solvay SIPOMER® PAM-300 Phosphate Esters of Ppg Monoacrylate
Solvay SIPOMER® PAM-100 Phosphate Esters of Polyethylene Glycol Monomethacrylate

WRHOD511 / 137742

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.