MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Eastman Cadence™ GS5 Clear (Unpigmented) Copolyester for film calendering
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Cadence™ GS5 is an amorphous copolyester with improved processability for film calendering. Calendered films made of Cadence™ copolyester are non-crystallizing, are halogen-free, offer wide calendering and thermoforming windows and have good low-temperature toughness. They are cooperative in secondary operations such as solvent-bonding, lamination, decoration, cold-forming, punching/cutting and embossment. Eastman Cadence™ resins require no pre-drying or additional stabilizers. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.

Application/Uses

  • Appliance films
  • Architectural laminates
  • Automotive films
  • Bags
  • Decorative laminates
  • Electronic laminates
  • Floor coverings
  • Furniture/Furniture trim
  • Labels
  • Outdoor films
  • Packaging
  • Printable films
  • Shrink film
  • Transaction cards
  • Transportation laminates
  • Wall coverings

Reported typical properties are preliminary. Information was provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83ASTM D2240
Secant Modulus, MD 1.87 GPaTangent; ASTM D882
Secant Modulus, TD 1.825 GPaTangent; ASTM D882
Film Tensile Strength at Break, MD 50.0 MPaASTM D882
Film Tensile Strength at Break, TD 48.0 MPaASTM D882
1% Secant Modulus, MD 1800 MPaASTM D882
1% Secant Modulus, TD 1760 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -45.0 °Cby Impact; ASTM D1790
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Descriptive Properties
Greenguard Indoor Air Quality Certifiedyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Cadence™ GS3 Copolyester for film calendering
Eastman Tritan™ GX100 Copolyester
Eastman Tritan™ MP100 Copolyester
Eastman Tritan™ MX710 Medical Grade Copolyester
Eastman Cadence™ GS5 Opaque White Copolyester for film calendering

PE8905 / 109247

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.