MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) solvene® 250 EAP Electroactive Polymer (EAP)  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Annealing Temperature - < 135 °C; Breakdown Voltage - 250 kV/mm; Coercive Field - 50 kV/mm; Crystallization Point - ASTM D3418 123 °C; Curie Temperature - ASTM D3418 110 °C; d33 - -38.0 pC/N; Kt - 35 %; Molecular Weight - ISO 16014-1 75 to 500; Poling Field - < 200 kV/mm; Remanent Polarization - < 10.0 µc/cm²

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 75 - 500 g/mol75 - 500 g/molISO 16014-1
Melt Flow 0.10 - 400 g/10 min0.10 - 400 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 49.0 - 54.0 MPa7110 - 7830 psiASTM D638
Tensile Strength, Yield 22.0 - 28.0 MPa3190 - 4060 psiASTM D638
Elongation at Break 400 - 600 %400 - 600 %ASTM D638
Elongation at Yield 9.0 - 12 %9.0 - 12 %ASTM D638
Tensile Modulus 0.550 - 0.850 GPa79.8 - 123 ksiASTM D638
 
Electrical PropertiesMetricEnglishComments
Curie Temperature 110 °C230 °FASTM D3418
Dielectric Constant 15
@Frequency 1e+6 Hz
15
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 144 °C291 °FASTM D3418
Crystallization Temperature 123 °C253 °FASTM D3418
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
FormPowder

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Eagle Brass 200/201 Nickel Alloy, Annealed
Nitinol - NiTi Shape Memory Alloy; Low-Temperature Phase
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
Overview of materials for Styrene-Butadiene Copolymer, SBC

PSOL8Y7305 / 177036

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.