MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SPS Guang Zhou REMAS™ 6001RM10 Flame-retarded PE masterbatch
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Characteristic: High content of flame retardant, little adding amount in processing, dispersing evenly in PE matrix, high property/price

Applications: It can be used to LDPE, HDPE, LLDPE, or MDPE for the flame retardance

Appearance: Nature color particle (white)

Information Provided by SPS (Guang Zhou) Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-2V-2
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
PP/6001RM10 Ratio1/10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase Multi-Flam™ 0107 HDPE Polyethylene
Ovation Polymers Nima™ HL 18400 HDPE
Multibase Multi-Flam™ 0901 HDPE Polyethylene
Multibase Multi-Flam™ 0803 LDPE NH Polyethylene
Multibase Multi-Flam™ 0801 LDPE Polyethylene

PSPS033 / 103388

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.