MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ovation Polymers Nima™ HL 18400 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: High Density Polyethylene - Halogenated FR compound with good impact resistance.

*All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.

Information provided by Ovation Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D792
Melt Index of Compound 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 15.0 MPa2180 psi50 mm/min; ASTM D638
Tensile Strength, Yield 18.0 MPa2610 psi50 mm/min; ASTM D638
Elongation at Break >= 50 %>= 50 %50 mm/min; ASTM D638
Tensile Modulus 0.400 GPa58.0 ksi50 mm/min; ASTM D638
Flexural Strength 16.0 MPa2320 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 0.320 GPa46.4 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.869 J/cm3.501 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam® FR PE JR 165 High Density Polyethylene (HDPE)
Multibase Multi-Flam™ 0107 HDPE Polyethylene
Multibase Multi-Flam™ 0103 HDPE Polyethylene
Multibase Multi-Flam™ 0901 HDPE Polyethylene
Multibase Multi-Flam™ 2103 HDPE Polyethylene

POVAT064 / 55776

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.