MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucobit Lucowax® 1700 Polyethylene Wax
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Lucowax is a polyethylene wax additive for the modification of bitumen or asphalt.

The addition of Lucowax reduces viscosity and penetration, while increasing water resistance, plasticity, and deformation resistance.

Information provided by Lucobit AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.700 - 0.900 g/cc0.0253 - 0.0325 lb/in³ISO 1183
Viscosity <= 4000 cP<= 4000 cPDIN EN ISO 3104
Ash <= 1.0 %<= 1.0 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 60.0 - 130 °C140 - 266 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Evateno® HM 728 EVA Hot Melt Copolymer
ExxonMobil Escorene™ UL 7511 Ethylene Vinyl Acetate Copolymer
ExxonMobil Escorene™ UL 7521 Ethylene Vinyl Acetate Copolymer
Arkema EVATANE® 20-20 Copolymer Ethylene - Vinyl Acetate
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer

PLUCO963 / 151029

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.