MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eneos PP/DYNARON®1320P Film
Categories: Polymer; Thermoplastic; Polypropylene (PP); Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 17.7 MPaJIS K7127
Film Tensile Strength at Yield, TD 14.7 MPaJIS K7127
Film Elongation at Break, MD 620 %JIS K7127
Film Elongation at Break, TD 850 %JIS K7127
Tensile Modulus 270 MPaTD
 280 MPaMD
Tensile Impact 9.00 J/cm
@Temperature -20.0 °C
 50.3 J/cm
@Temperature 0.000 °C
Elmendorf Tear Strength MD 81.6 g
Elmendorf Tear Strength TD 958 g
Film Tensile Strength at Break, MD 56.9 MPaJIS K7127
Film Tensile Strength at Break, TD 45.1 MPaJIS K7127
Heat Seal Strength 0.0380 lb/in
@Temperature 120 °C
 1.027 lb/in
@Temperature 130 °C
 
Optical PropertiesOriginal ValueComments
Haze 3.1 %JIS K7105
 
Descriptive Properties
CompositionPP/DYNARON®1320P

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSRC8207 / 295523

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.