MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eneos PP/DYNARON®1320P Film
Categories: Polymer; Thermoplastic; Polypropylene (PP); Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 17.7 MPa2570 psiJIS K7127
Film Tensile Strength at Yield, TD 14.7 MPa2130 psiJIS K7127
Film Elongation at Break, MD 620 %620 %JIS K7127
Film Elongation at Break, TD 850 %850 %JIS K7127
Tensile Modulus 0.270 GPa39.2 ksiTD
 0.280 GPa40.6 ksiMD
Tensile Impact  9.00 J/cm
@Temperature -20.0 °C
16.9 ft-lb/in
@Temperature -4.00 °F
 50.3 J/cm
@Temperature 0.000 °C
94.2 ft-lb/in
@Temperature 32.0 °F
Elmendorf Tear Strength MD 81.6 g81.6 g
Elmendorf Tear Strength TD 958 g958 g
Film Tensile Strength at Break, MD 56.9 MPa8250 psiJIS K7127
Film Tensile Strength at Break, TD 45.1 MPa6540 psiJIS K7127
Heat Seal Strength  17.2 g/25 mm
@Temperature 120 °C
0.0380 lb/in
@Temperature 248 °F
 465.8 g/25 mm
@Temperature 130 °C
1.027 lb/in
@Temperature 266 °F
 
Optical PropertiesMetricEnglishComments
Haze 3.1 %3.1 %JIS K7105
 
Descriptive Properties
CompositionPP/DYNARON®1320P

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJSRC8207 / 295523

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.