MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek TS-83 Thermoset Electrical Insulation Product (Nema Grade: LE)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: Linen reinforcement, Phenolic resin, Tan / Black color. Good electrical and high mechanical strength. Moisture resistant.

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³
Water Absorption 1.0 %1.0 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 152 MPa22000 psi
Compressive Strength 262 MPa38000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.00e+10 ohm-cm7.00e+10 ohm-cm
Dielectric Strength 14.0 kV/mm356 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
LE Phenolic Laminate
304 Stainless Steel
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast

PPYRO052 / 58385

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.