MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem INSPIRE™ 136 Performance Polypropylene Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade; Polypropylene, Extrusion Grade

Material Notes: Description: Braskem INSPIRETM 136 Performance Polymer is a low gel resin developed for the manufacturing of films for quality applications. Braskem INSPIRETM 136 Performance Polymer combines good processability with good stiffness and low gel content. It can be used as a blend partner to make more effective films with blown or cast film technology.

Application:

  • food packaging
  • hygiene applications

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 27.0 MPa
@Thickness 0.0500 mm
Blown Film; ISO 527-3
 35.0 MPa
@Thickness 0.0500 mm
Blown Film; ISO 527-3
Film Tensile Strength at Yield, TD 23.0 MPa
@Thickness 0.0500 mm
Blown Film; ISO 527-3
 30.0 MPa
@Thickness 0.0500 mm
Blown Film; ISO 527-3
Film Elongation at Break, MD 610 %
@Thickness 0.0500 mm
ISO 527-3
Film Elongation at Break, TD 650 %
@Thickness 0.0500 mm
ISO 527-3
Flexural Modulus 1150 MPaInjection Molded; ISO 178
Puncture Energy 3.00 J
@Thickness 0.0500 mm
ASTM D5748
 70.0 J
@Thickness 0.0500 mm
ASTM D5748
Elmendorf Tear Strength MD 27 g
@Thickness 0.0500 mm
ISO 527-3
Elmendorf Tear Strength TD 50 g
@Thickness 0.0500 mm
ISO 527-3
Dart Drop Test 170 g
@Thickness 0.0500 mm
ISO 7765-/A
1% Secant Modulus, MD 680 MPa
@Diameter 0.0500 mm
Blown Film; ISO 227-3
1% Secant Modulus, TD 650 MPa
@Diameter 0.0500 mm
Blown Film; ISO 227-3
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °CISO 72-2/B
Vicat Softening Point 151 °CIOS 306/A
 
Processing PropertiesOriginal ValueComments
Melt Temperature <= 230 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem INSPIRE™ 361 Performance Polypropylene Polymer
Braskem INSPIRE™ 114 Performance Polypropylene Polymer
Braskem INSPIRE™ 224 Polypropylene Homopolymer
Braskem INSPIRE™ 222 Performance Polypropylene Polymer
Braskem INSPIRE™ 216 Polypropylene Homopolymer

PBRASK2111 / 199992

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.