MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Braskem INSPIRE™ 361 Performance Polypropylene Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade

Material Notes: Description: INSPIRE™ 361 Performance Random Copolymer has been specifically developed for film extrusion applications. The polymer combines features like good processing, excellent mechanical property balance and high clarity.

Application:

  • Specialty film e.g. multilayer component
  • Shrink film

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Flow 1.8 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.8 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 47.0 MPa
@Thickness 0.0500 mm
6820 psi
@Thickness 0.00197 in
ISO 527-3
Film Tensile Strength at Yield, TD 32.0 MPa
@Thickness 0.0500 mm
4640 psi
@Thickness 0.00197 in
ISO 527-3
Film Elongation at Break, MD 580 %
@Thickness 0.0500 mm
580 %
@Thickness 0.00197 in
ISO 527-3
Film Elongation at Break, TD 280 %
@Thickness 0.0500 mm
280 %
@Thickness 0.00197 in
ISO 527-3
1% Secant Modulus, MD 810 MPa
@Diameter 0.0500 mm
117000 psi
@Diameter 0.00197 in
ISO 227-3
1% Secant Modulus, TD 790 MPa
@Diameter 0.0500 mm
115000 psi
@Diameter 0.00197 in
ISO 227-3
 
Optical PropertiesMetricEnglishComments
Haze 3.0 %
@Thickness 0.0500 mm
3.0 %
@Thickness 0.00197 in
Blown Films; ASTM D1003
Gloss 80 %80 %45°; ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem INSPIRE™ 136 Performance Polypropylene Polymer
Braskem INSPIRE™ 6025 Polypropylene Homopolymer
Braskem INSPIRE™ 6025N Polypropylene Homopolymer
Braskem INSPIRE™ 114 Performance Polypropylene Polymer
Braskem INSPIRE™ 224 Polypropylene Homopolymer

PBRASK2113 / 199994

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.