MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Polypropylene PPC 3666 is a heterophasic copolymer with a Melt Flow index of 1.5 g/10 min. This resin offers an outstanding processability in combination with good melt strength and excellent mechanical properties.

Polypropylene PPC 3666 has been especially developed for the extrusion of corrugated cardboard. It offers an excellent performance as well in other applications, include sheet and film extrusion and thermoforming.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.905 g/cc0.905 g/ccISO 1183
Bulk Density 0.525 g/cc0.0190 lb/in³ISO 1183
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7777ISO 2039-2
Tensile Strength, Yield 24.0 MPa3480 psiISO 527-2
Elongation at Yield 11 %11 %ISO 527-2
Tensile Modulus 1.30 GPa189 ksiISO 527-2
Flexural Modulus 1.20 GPa174 ksiISO 178
Izod Impact, Notched (ISO)  7.00 kJ/m²
@Temperature -20.0 °C
3.33 ft-lb/in²
@Temperature -4.00 °F
ISO 180
 >= 50.0 kJ/m²
@Temperature 23.0 °C
>= 23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Charpy Impact, Notched  0.800 J/cm²
@Temperature -20.0 °C
3.81 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 >= 5.00 J/cm²
@Temperature 23.0 °C
>= 23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C198 °F120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °F120°C per hour; ISO 752
Vicat Softening Point  60.0 °C
@Load 5.10 kg
140 °F
@Load 11.2 lb
50°C per hour; ISO 306
 130 °C
@Load 1.02 kg
266 °F
@Load 2.25 lb
50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet
Total PPC 7642 Polypropylene, Heterophasic Copolymer
Ineos N02J-00 Polypropylene Impact Copolymer
Total PPC 4481WZ Polypropylene, Impact Copolymer
Total PPC 4280W Polypropylene, Impact Copolymer

PTOTAL846 / 130571

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.