MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos N02J-00 Polypropylene Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: This is a low melt flow rate, high impact copolymer polypropylene for sheet extrusion and thick wall injection molding applications. It offers a superior balance of stiffness and impact strength for thermoformed articles where freezer to microwave performance is required. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

    Applications
  • Appliances
  • Compounding
  • Consumer products
  • Housewares
  • Rigid packaging

    Benefits
  • Enhanced room temperature and low temperature impact
  • Enhanced stiffness

Information provided by Ineos Olefins & Polymers USA

Key Words: Superior balance of stiffness and impact strength
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ASTM D792
Melt Flow 1.9 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.9 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090Injection Molded; ASTM D785
Tensile Strength at Break 17.1 MPa2480 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 28.9 MPa4190 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break 160 %160 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 5.4 %5.4 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 1580 MPa229000 psiInjection Molded; ASTM D790A
Izod Impact, Notched  0.747 J/cm
@Temperature -20.0 °C
1.40 ft-lb/in
@Temperature -4.00 °F
Injection Molded; ASTM D256
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
Injection Molded; ASTM D256
Izod Impact, Notched (ISO) 7.10 kJ/m²
@Temperature -20.0 °C
3.38 ft-lb/in²
@Temperature -4.00 °F
Area, Injection Molded; ASTM D256
Impact  NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
Instrument Dart Impact, Injection Molded, Ductile Failure; ASTM D3763
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
Instrument Dart Impact, Injection Molded, Ductile Failure; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C241 °FUnannealed, Injection Molded; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 61.1 °C142 °FUnannealed, Injection Molded; ASTM D648
Vicat Softening Point 153 °C307 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 59 %59 %60°, Injection Molded; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ProcessInjection Molding
 Sheet Extrusion
 Thermoforming

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos N02G-00 Polypropylene Impact Copolymer
Ineos N01N-00 Polypropylene Impact Copolymer
Ineos N20G-00 Polypropylene Impact Copolymer
Ineos N01G-02 Polypropylene Impact Copolymer
Ineos N00N-00 Polypropylene Impact Copolymer

PINEOS056 / 99377

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.