PSF-42 was developed by Navy subcontractors for simple shipyard-based cavity pours of Naval vessels. This system may be used in any free-flood cavity or void, but is especially valuable in difficult-to-fill cavities and in circumstances where quick working time is required. The mix is a low viscosity, multicomponent, fast cure system that cures at room temperature to form a solid syntactic material that will easily perform at depths of 1,500 feet. |